Resistivity in two traditions

Resistivity is a property of a material: how strongly it resists current, independent of the size of the sample. Metallurgists and conductor makers often use microohm meters or microohm centimeters, semiconductor engineers use ohm centimeters, and electrical engineers use ohm meters. This page converts from microohm meters to ohm centimeters. The default of 10 µΩ·m becomes 0.001 Ω·cm. The reason is simple. A micro prefix is 10⁻⁶, and a meter is 100 centimeters, so one µΩ·m is 10⁻⁶ ohm times 100 cm, which is 10⁻⁴ Ω·cm. The page multiplies by 0.0001 and leaves the material, its temperature and its condition to your source.

Resistivity versus resistance

Resistance and resistivity are related but different. Resistance, in ohms, belongs to a particular conductor and depends on its length and cross-section. Resistivity belongs to the material. The link is R = ρL/A, where ρ is resistivity, L is length and A is the cross-sectional area. Take ρ = 10 µΩ·m, which is 10⁻⁵ Ω·m, a conductor 2 m long and a cross-section of 1 mm², which is 10⁻⁶ m². Then R = 10⁻⁵ times 2 divided by 10⁻⁶, which is 20 Ω. The same material in a 1 m, 1 mm² sample has 10 Ω. The converter acts on ρ only. To get a resistance you need the geometry, and the formula above does the work. Mixing the two is a common source of unit errors, so label every number with its quantity. Writing the units out on every line of a calculation and cancelling them shows quickly whether the result is a resistance.

The factor and its derivation

Start from the definition of the units: 1 µΩ·m is 10⁻⁶ Ω·m. One meter is 100 centimeters, so 1 Ω·m is 100 Ω·cm, because resistivity grows with length units. Hence 1 µΩ·m is 10⁻⁶ times 100 Ω·cm, which is 10⁻⁴ Ω·cm. Multiplying 10 by 10⁻⁴ gives 0.001. The direction trips people up. Resistivity is ohms multiplied by a length, so the smaller length unit gives the larger number: the same material is 100 times bigger in Ω·cm than in Ω·m. The micro prefix then works the other way, shrinking the figure by a factor of one million. The net effect is a result in Ω·cm that is 10,000 times smaller than the number in µΩ·m.

Resistivities of familiar materials

Copper at 20 °C has a resistivity of about 0.0168 µΩ·m, and annealed copper under the IACS standard is 0.017241 µΩ·m. In ohm centimeters that is about 1.68 × 10⁻⁶ Ω·cm. Aluminum is about 0.0265 µΩ·m, or 2.65 × 10⁻⁶ Ω·cm. Iron is roughly 0.097 µΩ·m, and stainless steels run from about 0.7 to 0.8 µΩ·m. Nichrome, used in heating elements, is around 1.1 µΩ·m, which is 1.1 × 10⁻⁴ Ω·cm. The default 10 µΩ·m is far above the common metals and sits closer to the range of graphite and other carbon-based materials. These values are approximate textbook figures that vary with composition, temperature and processing. Use the manufacturer's data or a reference table for design work. The page converts units and does not supply material data.

Semiconductors and ohm centimeters

In semiconductor work, resistivity is almost always quoted in ohm centimeters. A silicon wafer might be specified as 1 to 10 Ω·cm for a typical doped substrate, while very high resistivity float-zone silicon may exceed 1,000 Ω·cm. Intrinsic silicon is around 2 × 10⁵ Ω·cm. Converting 1 Ω·cm to microohm meters gives 10,000 µΩ·m. The converter can do that in reverse, so an input of 10,000 µΩ·m returns 1 Ω·cm. Doping lowers resistivity by orders of magnitude, which is the point of doping. For metals, the equivalent numbers are tiny in ohm centimeters, and that is why metal data uses microohm units. The wide span from 10⁻⁶ Ω·cm for copper to 10⁵ Ω·cm for intrinsic silicon is one reason resistivity is plotted on logarithmic axes.

Water, soil and large resistivities

At the other extreme, insulators and ionic conductors have large resistivities. Ultrapure water has a resistivity of about 18.2 MΩ·cm at 25 °C, which is 1.82 × 10⁵ Ω·m. Seawater is near 0.2 Ω·m, or 20 Ω·cm. Soil resistivity, important for grounding design, ranges from tens to thousands of ohm meters depending on moisture and composition. A soil of 100 Ω·m is 10,000 Ω·cm. The converter supports ohm meters and ohm centimeters directly, so the pair 100 Ω·m and 10,000 Ω·cm can be checked on the page. Microohm meters do not suit these materials, since the numbers would be enormous, so engineers change units according to the range. Always write the unit with the value, since a bare 100 could mean any of these.

Ohm square millimeters per meter

Wire tables often list resistivity in ohm square millimeters per meter, written Ω·mm²/m. It is a convenient unit because it gives resistance per meter directly for a wire in square millimeters. Numerically it equals microohm meters: 1 Ω·mm²/m is 10⁻⁶ Ω·m, which is 1 µΩ·m. Copper is therefore 0.0168 to 0.0172 Ω·mm²/m. A conductor of 2.5 mm² then has about 6.9 mΩ per meter at 20 °C. The unit menu of the converter lists ohm square millimeters per meter, and converting 1 of them to microohm meters returns 1, which confirms the equality. Seeing the same number in different units helps students and technicians who move between data sheets from different regions. Cable standards generally list conductor resistance per kilometer, which follows the same arithmetic.

Microohm centimeters in metallurgy

Another common unit is the microohm centimeter, widely used in metals handbooks and materials science. One µΩ·cm is 10⁻⁸ Ω·m, so one µΩ·m equals 100 µΩ·cm. Copper at 0.0168 µΩ·m is 1.68 µΩ·cm, and aluminum at 0.0265 µΩ·m is 2.65 µΩ·cm. Those numbers are close to what a metallurgist would read from a handbook table. The unit menu includes microohm centimeters, and converting 0.0168 µΩ·m to them yields 1.68. The advantage of µΩ·cm is that common metals fall between about 1 and 100, which makes tables easy to scan. When comparing data from two sources, check whether one uses µΩ·m and the other µΩ·cm, because a factor of 100 can make an alloy look like a different material. A table of nichrome at 110 µΩ·cm and another at 1.1 µΩ·m describe exactly the same wire, and only the unit separates them. The page makes that comparison one step.

Temperature and measurement caveats

Resistivity depends on temperature, and a value without a temperature is incomplete. For copper, resistivity rises about 0.39 percent per kelvin near room temperature, so a value measured at 60 °C is about 15 percent higher than at 20 °C. Semiconductors behave the other way, with resistivity dropping as temperature rises in the intrinsic range. Measured resistivity also depends on purity, cold work and the measurement method, such as the four-point probe used on thin films and wafers. The converter does not correct for temperature and treats the input as a given. Always keep the temperature and condition of the sample with the number. Converting the unit does not change those conditions, and a table that mixes values at different temperatures can mislead in ways that no unit conversion can fix.

Frequent mistakes

Common errors include mixing up resistivity and conductivity, which are reciprocals. Conductivity is often given in siemens per meter or percent IACS, and the converter does not handle it. Another is mixing up resistivity and resistance, as described above. Third is the factor itself: multiplying by 10,000 instead of dividing, or using 100 for meters to centimeters when the micro prefix also applies. Fourth is the prefix: µΩ·m versus mΩ·m, a factor of a thousand. Quick checks help. Copper should come out near 1.7 × 10⁻⁶ Ω·cm, and a result of 17 or 0.017 for copper signals a slipped decimal. The relation 1 µΩ·m = 100 µΩ·cm = 10⁻⁴ Ω·cm is worth memorizing. Writing the full unit with every number takes seconds and avoids most of the trouble.

A heating wire worked through

Consider a nichrome heating wire with a resistivity of 1.1 µΩ·m, which the converter shows as 1.1 × 10⁻⁴ Ω·cm. The wire has a diameter of 0.5 mm, so its cross-section is pi times 0.25 squared, or 0.19635 mm². Resistance per meter is the resistivity in Ω·mm²/m divided by the area, which is 1.1 divided by 0.19635, or about 5.60 Ω per meter. A 2 meter length therefore has about 11.2 Ω at room temperature. Resistivity of nichrome changes only a little with temperature, which is one reason it is used for heaters, but the value in a real design should come from the alloy supplier. The numbers in this example are illustrative. They show how a resistivity from a handbook, in whatever unit it is printed, can be converted and then used with the geometry to give a resistance.

Scope of the conversion

The page restates one resistivity in another unit. It does not look up material data, correct for temperature, calculate wire resistance, size conductors or decide whether a material suits an application. Use handbook or supplier data for the number itself, and keep the original value, unit and temperature in your records so a later reader can check the step.

Thin films and sheet resistance

Thin-film work combines these units. Sheet resistance in ohms per square is resistivity divided by film thickness. For a copper film 1 µm thick with the bulk value of 0.0168 µΩ·m, the sheet resistance is 1.68 × 10⁻⁸ Ω·m divided by 10⁻⁶ m, or 0.0168 Ω per square. In the semiconductor convention the same numbers are 1.68 × 10⁻⁶ Ω·cm divided by 10⁻⁴ cm, which also gives 0.0168. Real thin films usually show higher resistivity than bulk metal, so the bulk figure is an illustration. The converter supplies the resistivity in the unit the film model expects.