Putting a handbook value into SI

Engineering software and physics formulas want resistivity in ohm meters. Handbooks, on the other hand, print values for metals in microohm centimeters. A solver for busbar heating, a thermal-electrical simulation or a coursework problem about wire resistance all ask for ρ in Ω·m, and typing 1.7241 into a field that expects 1.7241 × 10⁻⁸ gives an answer that is off by eight orders of magnitude. This page applies the factor of 10⁻⁸ and prints the SI value, so you can paste it straight into the model. Copper at 1.7241 µΩ·cm becomes 1.7241e-8 Ω·m, and aluminum at about 2.65 µΩ·cm becomes about 2.65e-8 Ω·m, the figures most textbooks list for 20 °C.

How the factor of 10⁻⁸ arises

Start from the definition of the units. 1 µΩ·cm is 10⁻⁶ Ω times 10⁻² m, which equals 10⁻⁸ Ω·m. Therefore Ω·m = µΩ·cm × 10⁻⁸. A common way to remember it is to take the value in µΩ·cm, divide by one hundred to reach µΩ·m, and then divide by one million to reach Ω·m. Two steps of a hundred and a million combine into a hundred million. If you use a calculator, enter the factor as 1E-8 and avoid typing a string of zeros, because miscounting zeros in 0.00000001 is easy. The page uses the same factor and returns the answer in plain decimal or scientific form depending on size.

The default of 10 µΩ·cm in ohm meters

The default of 10 µΩ·cm becomes 1e-7 Ω·m, written out as 0.0000001 Ω·m. A display may show 1e-7 or a long decimal that ends in a run of nines because of floating-point storage, which should be read as 1 × 10⁻⁷. The value is close to that of iron and nearly six times copper. In an SI model, that number means a one-meter length of conductor with a one-square-meter cross-section would have a resistance of 1e-7 Ω. Real conductors are far thinner, so the realistic resistance values come from dividing by the area, and the example below shows how that plays out for a bus bar. Note that a resistivity in Ω·m alone says nothing about how a part feels in use. It becomes meaningful only after you multiply by length and divide by area, and a thin or long conductor can reach a high resistance even from a modest resistivity.

Grounding rods and soil are a different scale

Earthing and grounding work also quotes resistivity in ohm meters, but the numbers there describe soil and run from tens to thousands of Ω·m, many orders above any metal. That is the same unit with a very different range, so a table of conductors and a table of soils cannot share an axis without a break. This page serves the metal end of the range. A copper rod at 1.7241e-8 Ω·m in a soil of 100 Ω·m is eight to ten orders of magnitude more conductive than its surroundings, which is why the rod resistance is negligible next to the soil resistance in a grounding calculation. For the metal side of such a design, a rod or strap, you still need the conductor resistivity in SI, and this page supplies it from a µΩ·cm table in one step.

A bus bar and a heating wire from the same table

Take an illustrative copper bus bar 2 m long with a 50 mm by 10 mm cross-section, which is 5 × 10⁻⁴ m². With ρ = 1.7241e-8 Ω·m, the resistance is ρL/A = 1.7241e-8 × 2 / 5e-4 = 6.8964e-5 Ω, about 69 µΩ. At a 500 A load the voltage drop is roughly 34 mV and the loss is about 17 W. Now take a nichrome heating wire at 110 µΩ·cm, which is 1.1e-6 Ω·m, 5 m long with a 0.5 mm² (5e-7 m²) section. The resistance is 1.1e-6 × 5 / 5e-7 = 11 Ω. Both results start from a handbook figure in µΩ·cm and finish after one conversion.

From resistivity to conductivity

In SI, conductivity is the reciprocal of resistivity and is measured in siemens per meter. Once the value is in Ω·m, the reciprocal follows directly. For copper, 1 / 1.7241e-8 is about 5.8 × 10⁷ S/m, or 58 MS/m, the number printed on many conductivity charts. Aluminum at 2.65e-8 Ω·m gives about 3.77 × 10⁷ S/m. Doing the reciprocal in microohm centimeters first, and converting afterward, invites the same factor error, so convert first and then invert. Eddy-current testing and induction heating references usually list conductivity in MS/m or percent IACS, and this conversion is the entry point for both.

Common slips with the exponent

Because the factor is so small, the usual errors come from the exponent. Typing 1.7241e-6 instead of e-8 makes the model copper 100 times too resistive. Using the µΩ·cm to µΩ·m factor of 0.01 by mistake leaves the answer a million times too large for an Ω·m field. Another slip is mixing centimeter-based area, such as 0.1 cm², with a resistivity in Ω·m, which silently produces nonsense. A sanity check is to compare your final resistance with a rule of thumb. Copper wire of 1 mm² and 1 m has about 17 mΩ, which is 0.017 Ω. If your number is far from that, check the exponent first.

Temperature coefficient and operating conditions

Handbook resistivity is quoted at a reference temperature, usually 20 °C. A conductor that runs hot has a higher resistivity, and for copper the increase is roughly 0.39 percent per degree Celsius near room temperature. A bus bar at 80 °C is therefore about 23 percent more resistive than the table value, which matters for loss and temperature rise calculations. Convert the handbook value with this page first, then apply the temperature correction in SI. Keep the reference temperature with the number in your model so a collaborator does not apply the correction twice or skip it. The page itself does not alter the value for temperature.

What the converter does not cover

The page converts the unit of resistivity. It does not calculate the resistance of a conductor, check current ratings or model skin effect at high frequency, where AC resistance exceeds the DC value computed from ρ. It also cannot judge whether a value is plausible for a material. A result of 1e-7 Ω·m is reasonable for steel and unreasonable for copper, and only you know which one you meant. Values are rounded only by floating-point storage, so the conversion itself is exact. For other combinations of ohm, centimeter and meter prefixes, use the related converters in this family.