Coercivity columns in kOe and kA/m
Permanent magnet suppliers often print two columns for the same property. One gives the coercivity in kilooersteds, the other in kiloamperes per meter. Engineers who work in SI, or who run simulations, take the kA/m number, while a technician with an older gaussmeter may think in oersteds. This page converts oersteds to kA/m so that a number from either column, or from a paper, can be moved to the unit you need. It is useful for anyone who selects magnets, checks a data sheet against a design requirement or builds a model whose inputs must be in SI units.
One over four pi, scaled by a thousand
The oersted is 1,000/(4π) A/m. Dividing by 1,000 turns that into kA/m, so 1 Oe equals 1/(4π) kA/m, which is 0.0795774715459 kA/m. The formula is kA/m = Oe × 0.0795774715459. The factor includes π, so the decimal form is cut at a finite number of digits. NIST SP 811 lists both units. A convenient memory aid is that 1 kOe is close to 79.6 kA/m, and 1 kA/m is about 12.57 Oe. Oersteds to kA/m divides by about 12.6, so any answer above the input comes from swapped menus. Keep the unit in the column header.
Ten oersteds is 0.796 kA/m
The default of 10 Oe returns 0.7957747154594768 kA/m. In a report you would write 0.796 kA/m. The value is small because 10 Oe is a weak field, well below the coercivity of any magnet used in practice. A more typical input is a few thousand oersteds. For small inputs the answer has a leading zero, and it may be easier to read in A/m, where the same field is 795.8 A/m. Pick the unit that places the figure between 1 and 1,000, and keep the same unit across a whole column so that grades can be ranked at a glance. The page offers both A/m and kA/m, so you can switch when the number looks awkward, and the underlying conversion is the same.
Twelve kilooersteds in kA/m
Sintered neodymium magnets are sold in grades whose intrinsic coercivity runs from roughly 12 kOe to over 30 kOe. Take a grade listed with 12 kOe, which is 12,000 Oe. The page returns 954.9297 kA/m. A data sheet that lists 955 kA/m for the same grade confirms the pair. The numbers are an illustration of the conversion, and the actual coercivity of a given product comes from the supplier, at a stated temperature. Comparing grades is much easier when all values are in one unit, so convert the whole table, and keep a column with the original value so that errors can be traced. A supplier that lists 955 kA/m for a 12 kOe grade has rounded the conversion to three digits, and your own figure of 954.9 kA/m is consistent with it. Differences at the fourth digit between suppliers usually come from rounding rules, not from different materials.
Ferrite magnets at a few thousand oersteds
Ceramic ferrite magnets have lower coercivity than the rare earth types, and data sheets often list values near 3,000 Oe or a little higher for common grades. As an illustration, 3,000 Oe converts to 238.7324 kA/m. A designer who must keep a magnet from demagnetizing in a motor compares the opposing field in the application, expressed in kA/m from a simulation, with the coercivity of the magnet. Both need the same unit before the comparison means anything. Remember that coercivity of ferrite falls at low temperatures and that of neodymium falls at high temperatures, so the temperature on the data sheet matters as much as the unit.
From kA/m back to oersteds
To read a simulation result on an oersted scale, choose kA/m as the source and oersteds as the target. A field of 800 kA/m is 10,053.1 Oe, which is about 10.05 kOe, and 1 kA/m is 12.56637 Oe. The page divides by 0.0795774715459, so the answer is larger than the input. This direction suits a person who has a requirement in SI, such as a demagnetizing field of 800 kA/m in a motor design, and who wants to compare it with the kOe values in a catalog. Round at the end, keeping the digits that match the precision of the requirement. A requirement of 800 kA/m written with two significant digits should be read as 10 kOe, not as 10,053 Oe, since the extra digits were never part of the requirement.
Hcb and Hcj are different columns
A magnet data sheet often lists two coercivities. The normal coercivity, written Hcb, is the reverse field at which the flux density B falls to zero. The intrinsic coercivity, written Hcj, is the reverse field at which the magnetization M falls to zero, and it is higher. Both can be given in kOe and kA/m, and converting one does not give the other. Use Hcj when judging whether a magnet will resist demagnetization permanently, and use the column your design method asks for. Whichever number you enter is rescaled without any knowledge of which coercivity it is, so label your values carefully.
Temperature and the stated conditions
A coercivity figure belongs to a temperature, usually 20 degrees Celsius unless the data sheet says otherwise. For neodymium magnets the coercivity falls as the temperature rises, which is why high grades with a suffix for temperature class exist. Converting the unit does not change this behavior. If you compare a figure for a hot motor with a figure at room temperature, the unit conversion is correct and the comparison is still wrong. Write the temperature next to the converted value, and use the supplier curves for the operating point of your design.
Checking supplier curves at the operating temperature
Simulating a magnetic circuit, judging whether a magnet will demagnetize, predicting a flux density and accounting for temperature and geometry belong to the data sheet and your simulation. Use the converter to keep units consistent between a catalog written in kOe, a simulation written in kA/m and a measurement written in A/m or Oe. Keep the original values in your notes, because a rounded number that goes through several conversions can drift slightly. Before you order magnets or sign off a drawing, check the converted figures against the supplier curve at the operating temperature, and ask which of the two coercivity columns a given requirement refers to. Round the final kA/m value only once.