Metals and semiconductors on one axis

Semiconductor engineers quote silicon wafers in ohm centimeters. A lightly doped wafer might be specified at 1 to 10 Ω·cm, a heavily doped one at 0.001 Ω·cm. Metallurgists quote copper, aluminum and silver in microohm centimeters, with values near 1.7, 2.7 and 1.6. Putting a metal, a silicide contact and a doped substrate on one chart requires a single unit, and the common choice is Ω·cm because it keeps semiconductor numbers readable. This page converts the metal side. Copper at 1.7241 µΩ·cm becomes 0.0000017241 Ω·cm, and a doped silicon value of 0.001 Ω·cm equals 1,000 µΩ·cm, which shows silicon at its most conductive is still hundreds of times more resistive than a metal.

The shift of six decimal places

Because the length unit is the same on both sides, only the prefix changes. A microohm is 10⁻⁶ ohm, so Ω·cm = µΩ·cm × 0.000001. Move the decimal point six places to the left. A value of 250 µΩ·cm becomes 0.00025 Ω·cm, and 40,000 µΩ·cm becomes 0.04 Ω·cm. There is no unit trap hiding in the length here, which separates this page from the µΩ·cm to µΩ·m conversion. The risk is the opposite: with six places to move, a decimal point slipped by one place goes unnoticed. If your result looks ten times too large or small, count the places again, or use the check below that anchors copper at 1.7241 µΩ·cm.

The default of 10 µΩ·cm

The page starts at 10 µΩ·cm and prints 0.00001 Ω·cm, which is 10⁻⁵ Ω·cm. The long string of nines sometimes shown, 0.000009999999999999999, is floating-point noise and means 0.00001. As a material, 10 µΩ·cm is typical of titanium disilicide in its low-resistivity phase, which process engineers quote at about 13 to 16 µΩ·cm, and it is close to the value for iron. Those values explain why silicide layers are laid over polysilicon gates and contacts: they cut resistance by a large factor compared with doped silicon itself. The converter does not know the material, so use the number only for what the source states.

Bulk resistivity from a measured resistor

Resistivity in Ω·cm is easy to measure on a bar of known geometry. Take a 2 cm long, 0.1 cm² section of a sintered conductive paste with a measured resistance of 0.0005 Ω. Its resistivity is R × A / L = 0.0005 × 0.1 / 2 = 0.000025 Ω·cm. Entering the answer as microohm centimeters shows 25 µΩ·cm after the reverse conversion, a believable value for a silver-filled paste, since cured pastes usually sit well above bulk silver at 1.59 µΩ·cm. The same geometry in meters would need conversions of both length and area, which is why many labs measure in centimeters first and convert only at the end using this page.

Resistivity and conductivity in practice

Conductivity is the reciprocal of resistivity. Ohm centimeters invert to siemens per centimeter, and microohm centimeters invert to mega-siemens per meter after a factor. For copper, 1 / 0.0000017241 Ω·cm is about 580,000 S/cm, or 58 MS/m, the figure behind the International Annealed Copper Standard, which defines 100 percent IACS as 1.7241 µΩ·cm at 20 °C. A conductor rated 61 percent IACS has a resistivity near 2.83 µΩ·cm. Converting to Ω·cm first is useful when a plating or coating specification states conductivity in S/cm, the common unit in electrochemistry and ionic conductors. Keep the arithmetic in one unit and invert only once at the end.

Spotting units in a mixed datasheet

Datasheets sometimes print Ω·cm and µΩ·cm in the same table, one for the substrate and one for the metal layer. The symbol µ can turn into u in plain-text exports, and the dot between Ω and cm sometimes disappears, which leaves "Ωcm" or "ohm-cm". A value of 0.0017 under a header that reads mΩ·cm is another variant, equal to 1.7 µΩ·cm. When a number looks wrong by exactly a factor of a thousand, suspect a milli versus micro confusion before suspecting the measurement. Convert each entry to Ω·cm with this page, and the table can be sorted without worrying about the prefix on each row.

Choosing precision for tiny results

Results such as 0.0000017241 Ω·cm carry many leading zeros, which invites transcription errors. Scientific notation, 1.7241 × 10⁻⁶ Ω·cm, is easier to copy correctly and keeps the significant digits visible. The number of significant digits should match the source. If a handbook gives copper as 1.68 µΩ·cm, quote 1.68 × 10⁻⁶ Ω·cm and avoid dressing it up with extra digits. This matters when you propagate values into a model, since extra digits suggest precision that the measurement of a film or wire never had. Keep the original microohm centimeter value beside the converted one so a reader can verify the step quickly. A short note on the measurement temperature, usually 20 °C or 25 °C, belongs in the same row of the table.

Contact resistance versus bulk resistivity

Technicians who probe a metal film or a plated pad sometimes confuse resistivity with contact resistance, and the units show why they differ. Resistivity belongs to the material and is stated in Ω·cm or µΩ·cm. Contact resistance belongs to an interface and is stated in ohms or in Ω·cm² for a specific contact area. A silicide contact specified at 1 × 10⁻⁷ Ω·cm² is a different kind of number from a silicide film resistivity of 15 µΩ·cm, which is 0.000015 Ω·cm after conversion here. Only the second can be converted with this page. If a datasheet places both in one table, check the unit column carefully before you enter anything, and keep the contact figures out of the resistivity list. Mixing them is a frequent source of review comments in process documentation, because the two quantities share the symbol ρ in some papers and a reader may assume they are interchangeable.

What the page leaves to you

The page performs a unit change. It does not tell you the material, the temperature or the measurement method behind the value, and resistivity of thin films depends strongly on thickness, grain size and processing. It also does not compute resistance of a sample, which needs length and area, or sheet resistance, which needs thickness. Use the related converters for other length bases, and record the source and conditions next to each number. The conversion itself is exact, because it is a power of ten, and any differences you see against a reference table come from rounding of the entered value.